Most failed prints aren't the printer's fault — the part simply wasn't designed for how an FDM printer works. These twelve rules cover almost everything that goes wrong.

Size and thickness

  1. Make walls a multiple of your line width. With a 0.4 mm nozzle, 0.8, 1.2 or 1.6 mm walls print as clean, solid lines. A 1.0 mm wall leaves a weak gap or gets filled with zig-zags.
  2. Nothing thinner than two lines. Features under about 0.8 mm (with a 0.4 mm nozzle) may not print at all. FabMake's Print check warns you about thin parts.
  3. Text needs strokes of 0.5 mm or more. For embossed or engraved text, use bold letters at least 4–5 mm tall and 0.6–1 mm deep.

Overhangs and bridges

  1. The 45° rule. Each layer can stick out a little past the one below. Up to about 45° from vertical prints fine without support; steeper needs support or a different orientation. FabMake's Print check colours overhangs orange and red.
  2. Bridges are fine — if they're short. A flat ceiling between two supports prints well up to 10–20 mm in PLA. Longer bridges sag.
  3. Use chamfers instead of fillets underneath. A rounded bottom edge starts as a 90° overhang; a 45° chamfer prints cleanly. Use rounded fillets on top edges, where they print perfectly.
  4. Give horizontal holes a teardrop or diamond top. Round holes lying on their side have a flat ceiling at the top. A pointed top avoids supports and keeps them round.

Fit and accuracy

  1. Leave clearance between moving parts: about 0.2–0.3 mm per side for parts that slide, 0.1 mm for press fits. See tolerances.
  2. Chamfer the bottom edge 0.3–0.5 mm to hide elephant's foot (the slightly wider first layer).

Strength and orientation

  1. Layers are the weak direction. Parts break between layers, so orient them so the force runs along the layers. A hook printed standing up snaps; the same hook printed lying flat is strong.
  2. Walls matter more than infill. For strong parts, add walls (3–4) before raising infill. 15–20 % infill is enough for most things.
  3. Big flat parts warp. Round the corners (a 3–5 mm radius helps a lot), and avoid sharp corners on large ABS/ASA prints.

Make it easy to print

  • Put the biggest flat face on the plate. FabMake's Lay on a face does this in one click.
  • Split parts that would need lots of support into two pieces with alignment pins or a dovetail.
  • Add a fillet where a thin feature meets a thick one — it removes the weak spot.
Design it in FabMake